ExxonMobil Label-Lyte® 85 LP-200M Mirror Finish, Metallized, Whit Opaque OPP for Water-based Patch Label Applications
Subcategory: Adhesive; Polypropylene; Thermoplastic; Polymer
Material Notes: White, polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. It has an anti-static, "mirror finish" metallized print surface that is corona treatable for printing. This film is compatible with water-based or solvent-based flexo and gravure inks and UV-cured inks. It is designed to be used as a monoweb and provides excellent converting performance, including printing, sheeting, guillotine cutting, and label transfer on magazine-fed labelers, such as Krones Topmatic labeling equipment. Information provided by ExxonMobil Chemical
| Available Properties |
- Thickness
- Coating Weight
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Transmission, Visible
- Gurley Stiffness, MD, mgf
- Gurley Stiffness, TD, mgf
- Yield, in2/lb
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|