ExxonMobil Digilyte® 65 EW-214 Coated, White Opaque OPP Facestock
Subcategory: Adhesive; Polypropylene; Thermoplastic; Polymer
Material Notes: White, polypropylene, pressure-sensitive, label facestock designed to be printed on an Indigo® Omnius® One-Shot Color™ press. This film offers strength and opacity. The ElectroInk® receptive coating assures excellent anchorage and improved abrasion resistance with the ElectroInk digital printing inks. The opposite surface is coated to provide excellent pressure-sensitive adhesive adhesion. Information provided by ExxonMobil Chemical
| Available Properties |
- Thickness
- Coating Weight
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Transmission, Visible
- Gurley Stiffness, MD, mgf
- Gurley Stiffness, TD, mgf
- Yield, in2/lb
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|