ExxonMobil ESCOREZ™ 1102 Petroleum Hydrocarbon Resin
Subcategory: Adhesive; Additive/Filler for Polymer
Material Notes: Aliphatic hydrocarbon resin which is designed to tackify a variety of adhesive polymers including APP, APAO, natural rubber, synthetic polyisoprene, polyisobutylene and butyl rubber. Information provided by ExxonMobil Chemical
| Available Properties |
- Specific Gravity
- Brookfield Viscosity
- Molecular Weight
- Ash
- Acid Value
- Glass Temperature
- Ring & Ball Softening Point
- Gardner Color Number
- Chloride Content, ppm
- EVA/Resin/Wax Cloud Point, C
|
|
|
|