ExxonMobil ESCOREZ™ 1315 Petroleum Hydrocarbon Resin
Subcategory: Adhesive; Additive/Filler for Polymer
Material Notes: Premium aliphatic hydrocarbon resin with a high softening point. It is designed to provide high temperature performance and cohesive strength with a variety of adhesive polymers including APP, APAO, natural rubber, synthetic polyisoprene, polyisobutylene, and butyl rubber. Information provided by ExxonMobil Chemical
| Available Properties |
- Specific Gravity
- Brookfield Viscosity
- Molecular Weight
- Ash
- Acid Value
- Glass Temperature
- Ring & Ball Softening Point
- Gardner Color Number
- Chloride Content, ppm
- EVA/Resin/Wax Cloud Point, C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|