ExxonMobil ESCOREZ™ 2510 Petroleum Hydrocarbon Resin
Subcategory: Adhesive; Additive/Filler for Polymer
Material Notes: Premium aromatic modified aliphatic resin with a narrow molecular weight distribution. Characterized by low color, lo volatility, and low odor. It is designed for tackification of SIS block copolymers, but also has utility in natural rubber, polyisobutylene, butyl rubber, EVA, APP and APAO. Information provided by ExxonMobil Chemical
| Available Properties |
- Specific Gravity
- Brookfield Viscosity
- Molecular Weight
- Ash
- Collected Volatile Condensable Material
- Acid Value
- Glass Temperature
- Ring & Ball Softening Point
- Gardner Color Number
- Chloride Content, ppm
|
|
|
|
| Property Data |