ExxonMobil ESCOREZ™ 5637 Petroleum Hydrocarbon Resin
Subcategory: Adhesive; Additive/Filler for Polymer
Material Notes: Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers. Information provided by ExxonMobil Chemical
| Available Properties |
- Specific Gravity
- Brookfield Viscosity
- Molecular Weight
- Ash
- Acid Value
- Glass Temperature
- Ring & Ball Softening Point
- Gardner Color Number
- Aromacity, %
|
|
|
|