ExxonMobil EXXELOR™ VA 1803 Maleic anhydride functionalized elastomeric ethylene copolymer
Subcategory: Polyethylene; Elastomer, TPE; Additive/Filler for Polymer
Material Notes: High Flow, amorphous ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone results in outstanding thermal and oxidative stability leading to enhanced weatherability. Moreover, its amorphous nature exhibits impact resistance at very low temperatures in blends engineering polymers such as polyamide. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Melt Flow
- Collected Volatile Condensable Material
- Glass Temperature
- Yellow Index
- Maleic anhydride graft level
|
|
|
|
| Property Data |