ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene
Subcategory: Elastomer, TPE; Polypropylene; Additive/Filler for Polymer
Material Notes: Maleic anhydride functionalized polypropylene copolymer, produced by reactive extrusion. Primarily designed to add polarity to polypropylene matrices and in particular improve polypropylene reactivity with amino-silane treated glass reinforcements. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Melt Flow
- Collected Volatile Condensable Material
- Melting Point
- Yellow Index
- Maleic anhydride graft level
|
|
|
|
| Property Data |