ExxonMobil Escorene® HD-6704 HDPE, Injection Grade
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: High Density Polyethylene; Exxon Chemical Canada
Material Notes: Data Provided by Exxon Chemical Canada.Characteristics: Excellent Toughness, Excellent Stiffness, Excellent ESCR Uses: Industrial containers, Industrial lids
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Linear Mold Shrinkage
- Melt Flow
- Spiral Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Melting Point
- Brittleness Temperature
- Processing Temperature
|
|
|
|