ExxonMobil Escorene® HD-8760 HDPE, Rotational Molding Pellets
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: High Density Polyethylene; Exxon Chemical Canada
Material Notes: Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated UV-8 type protection, Higher stiffness, Good flow Uses: Recreational products, Industrial components, RV tanks
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |