ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit superior impact strength, good heat sealability and good low temperature properties. Applications: Frozen food packaging; Other food packaging including poultry bags, produce bags, etc.; Other packaging applications where excellent toughness and good heat sealability are required. Data for film properties below based on 1.25 mil film.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Dart Drop Test
- Melting Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|