ExxonMobil Escorene® LD-725 High EVA Film and Compounding Resin
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. An 18% vinyl acetate copolymer designed for specialty film and compounding applications. Outstanding sealability and low modulus are key attributes of products produced with this resin. Excellent filler acceptance produces highly loaded concentrates. Applications: Compounding; Electrical; Concentrates; Heat seal layer in coextruded or laminated structures.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|