ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and neck-in and can be coextruded with homopolymer extrusion coating resins on most coextrusion coating lines. Applications: Heat seal layer for cheese packaging; Other extrusion coating applications requiring outstanding heat sealability; Sealing layers requiring improved caulking. Data for film properties below based on 1.25 mil film.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact Test
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Melting Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|