ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding
Subcategory: Ethylene Methyl Acrylate; Thermoplastic
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: EMA; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. 23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It can also be used in coextrusions where adhesion and thermal processing stability are required or as an elastic, tough monolayer film. Applications: Compatibilizer and impact modifier for engineering thermoplastics; Coextruded tie layer for flexible packaging applications.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|