ExxonMobil Optema® TC-114 Ethylene Methyl Acrylate for Blown Film
Subcategory: Ethylene Methyl Acrylate; Thermoplastic; Polymer
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: EMA; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. 18% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elastic film with good handling characteristics without additional additives. Applications: Upholstery film; Disposable gloves; Hospital drapes. Data for film properties below based on 1.25 mil film.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Dart Drop
- Melting Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|