ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification
Subcategory: Ethylene Methyl Acrylate; EMAAA Terpolymer; Thermoplastic
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Ethylene Acid Terpolymer; ; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. 45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, etc. Applications: High end-use temperature adhesive; Engineering thermoplastic modifier; Heat activated sealant; Adhesion of dissimilar materials such as elastomers to metals.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Vicat Softening Point
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|