ExxonMobil Iotek® 7510 Zinc Ionomer Molding/Extrusion Resin
Subcategory: Ionomer; Thermoplastic
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A "soft" zinc ionomer with excellent flexibility and impact strength. This ionomer has outstanding adhesion to glass, metals and paper. IOTEK ionomers provide superb low temperature impact strength when blended with other polymers. Applications: Golf ball covers; Injection molded articles; Impact modifiers; Flexible tubings.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|