ExxonMobil Escorene® HD-8661 LHDPE Rotational Molding Grade
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Linear High Density Polyethylene; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. HD-8600 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8661 is fully formulated long term UV stability package in ground form. Applications: Large agricultural tanks; Industrial products.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Impact Test
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|