ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: High Density Polyethylene; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recommended for films 0.5 mil or greater in thickness. Applications: Oriented film products; Box liners; Protective packaging; Deli wrap. Data for film properties below based on 0.5 mil film.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|