ExxonMobil Escorene® LL-5102 LLDPE Compounding Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Linear Low Density Polyethylene; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL-5102 makes for efficient blending with pigments, slip additives and antiblock additives. Applications: Color concentrates; Slip and antiblock masterbatches.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Dart Drop, Total Energy
- Melting Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|