ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 0.5 mil Film
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Low Density Polyethylene
Material Notes: Data provided by the manufacturer, Exxon Chemical. A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges. Applications: Dry cleaning establishment bags; Protective garment bags; Other film applications requiring drawdown to 0.5 mil or below. Data for film properties below based on 0.5 mil film.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Dart Drop Test
- Melting Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|