ExxonMobil Escorene® LD-129 MDPE Cast Overwrap Film Resin
Subcategory: Polyethylene; Thermoplastic; MDPE; Polymer
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Medium Density Polyethylene; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-129 can be used in overwrap applications and in push-through type packaging equipment. LD-129 is suitable for processing in chill roll casting equipment. Applications: Bakery product overwrap; Soft goods (paper products) overwrap; Film is particularly suitable for applications requiring stiffness, crispness, machinability and abrasion resistance. Data for film properties below based on 1.25 mil film.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Dart Drop Test
- Melting Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|