ExxonMobil Escorene® LD-203 LDPE Extrusion Coating for Milk Cartons, High Speed
Subcategory: Polyethylene; Thermoplastic; LDPE
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Low Density Polyethylene; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A low density polyethylene resin with excellent adhesion, drawability and heat sealability. LD-203 also exhibits excellent barrier properties and grease resistance. Applications: Milk cartons; Board stock; Multiwall bag coating; Flexible packaging structures.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Melt Flow
- Seal Strength
- Melting Point
|
|
|
|