ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications. Applications: Designed to be blended with a suitable masterbatch to provide a crosslinkable low voltage cable insulation compound.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Melting Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|