ExxonMobil Escorene® LD-421 LDPE Power Cable Insulation
Subcategory: Polyethylene; Thermoplastic; LDPE
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Low Density Polyethylene; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A crosslinkable polyethylene homopolymer designed as an electrical grade base resin. Applications: A base resin for fully formulated crosslinkable medium voltage cable insulation compounds.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Melting Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|