ExxonMobil Escomer® H-101 Low MW HDPE Wax
Subcategory: Polyethylene; Thermoplastic; HDPE
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: High Density Polyethylene; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. A low molecular weight synthetic polyethylene wax with a unique combination of high drop point and extreme hardness coupled with an exceptionally low melt viscosity. Applications: Hot melt adhesives; Rubber processing aid; Pigment dispersion; Candles.
| Available Properties |
- Density
- Viscosity
- Melting Point
|
|
|
|
| Property Data |