ExxonMobil Exact® 3017 Plastomer for Specialty Applications
Subcategory: Polyethylene; Elastomer, TPE; Thermoplastic
Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.
Key Words: Polyethylene; Elastomer, Thermoplastic TPE; Exxon Chemical Company
Material Notes: Data provided by the manufacturer, Exxon Chemical. An ethylene-based plastomer produced using Exxon Chemical's EXXPOL Technology. The resin is designed for specialty applications requiring high flow. The resin is supplied with a primary antioxidant for protection against thermal oxidation.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Impact Test
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|