Expancel® 950 MB 80 Masterbatch with unexpanded microspheres
Subcategory: Additive/Filler for Polymer
Material Notes: Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the thermoplastic shell softens and the gas increases its pressure, resulting in an expansion of the spheres.Applications:
| Available Properties |
- Bulk Density
- Carrier
- Height of Foaming, mm
- Microsphere Content, %
|
|
|
|
| Property Data |