Fibre Glast 2000 / 2120 System 2000 Epoxy

 

Subcategory: Epoxy; Thermoset

Material Notes:
System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical properties of carbon fiber, Kevlar®, and glass laminates! Test results have proven superiority over other room temperature epoxies. Its low viscosity and great handling characteristics make it a favorite in the shop too!

Three high performance hardener systems are available for the System 2000 resin. 20 minute, 60 minute, and 120 minute pot life versions are all options. This added variety allows the fabricator to select the system best suited to the size, complexity or time-frame of the project. Simple parts which need to be demolded quickly should use the 20 minute hardener. Larger and more complex parts can use either of the other hardeners.

Vacuum bagging applications would typically warrant the longest 2 hour working time. As with any epoxy system, adhere to the proper mix ratios and maintain an adequate curing temperature of at least 70°F. The cure time will be cut in half for every 10°F that the temperature is raised above 70°F.

The long pot life 2120 hardener extends working time on large-scale and complex projects. Suitable for vacuum bagging and laminating in hot climates. The 24-36 hour demold time can be reduced by increasing the cure temperature. The post cured service temperature exceeds 200°F.

Information provided by Fibre Glast Developments Corporation.

Available Properties
  • Density
  • Viscosity
  • Hardness, Shore D
  • Tensile Strength @ Break
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • CTE, linear 68°F
  • Glass Temperature
  • Pot Life
  • Color
  • Mix Ratio
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。