Fibre Glast 1099 Room Temperature Epoxy Surface Coat
Subcategory: Epoxy; Thermoset
Material Notes: Safety hardener with fast overnight cure. Low viscosity thins the resin well for best detail reproduction. Can be sanded in 16-18 hours. #1099 is a white, medium viscosity epoxy surface coat that can be used with several hardeners for a range of cured and handling characteristics. #1099 is a versatile material, and will perform well in a variety of room temperature applications. #1099 produces excellent reproduction of very fine detailed surfaces. it is often chosen for broad, flat tooling surfaces, where it can be applied fast. #1099 has been formulated to provide good bonds to subsequently applied layers of epoxy. This feature provides good intercoat bonds, even if the previous layer of #1099 has cured completely hard. This elimination of surface coat adhesion failures is accomplished with no sacrifice in properties. #1099 is an excellent material for all types of general tooling uses. Information provided by Fibre Glast Developments Corporation.
| Available Properties |
- Hardness, Shore D
- Tensile Strength @ Break
- Flexural Strength
- Compressive Yield Strength
- Cure Time
- Pot Life
- Color
- Mix Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|