Fibre Glast 1100 Light-Weight High-Strength Patching/Filler Compound
Subcategory: Epoxy; Thermoset
Material Notes: Product Features:
- Very Light Weight Material
- Non-Hazardous Product - Safe to Use
- Easily Sanded and Carved with Shop Tools
- Negligible Shrinkage
- Non-Critical, 2 to 1 Ratio by Weight or by Volume
- Excellent Non-Sag Properties - Even Upside Down
- Slightly Flexible Cure - Not Brittle in Thin Sections
- Excellent Adhesion to a Variety of Surfaces
- Stable Formula - No Separation of Components in Storage
Description: #1100 is a two-component paste epoxy patching and filler compound for foam, wood, fiberglass, and other surfaces. The mixed consistency of this system is very smooth and creamy, so it spreads easily, and can be splined to a feather edge without separation. It is a thixotropic, non-sag material that will remain in place in thick sections, even when applied upside down. The resin and hardener of this system are color coded for easy mixing. The resin is white and the hardener is brown, giving a good visual indication of complete mixing with a uniform tan color free of streaks. #1100 has special low density fillers incorporated into it that provide very distinct benefits. It is a very light material (4 pounds per gallon), and therefore contributes minimal added weight to the filled or repaired structure. Also, the cured material is very easy to sand, making the finished patch undetectable when covered or painted. There are no volatile ingredients in #1100, so the cured material will not outgas, which could cause a loss of adhesion of paint or coverings. #1100 is not corrosive to metals, and will not promote corrosion on these surfaces, so bond line stability and long term adhesion are excellent. #1100 is a non-toxic material. There are non hazardous or restricted raw materials in either the resin or hardener of this system. Information provided by Fibre Glast Developments Corporation.
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore D
- Compressive Yield Strength
- Cure Time
- Pot Life
- Gel Time
- Color
- Mix Ratio
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|