Fibre Glast 77 Wax-Free General Purpose Polyester Molding Resin
Subcategory: Polyester, TS; Thermoset
Material Notes: Description:#77 Molding Resin is ideal for general purpose part fabrication and for building low cost molds. An internal thickening agent has been added to prevent drainage on vertical surfaces, yet it retains the low viscosity required for rapid wet out. This resin is wax free to reduce sanding between coats. #77 Polyester Molding Resin is a prepromoted, thixotropic, general purpose resin.
Performance:- High thixotropic index to prevent draining on vertical surfaces
- Low viscosity fir fast wet-out
- Styrene suppressed
Suggested Uses:#77 Polyester Molding Resin can be used for hand lay-up or spray-up for general fiberglass reinforced plastics applications. Information provided by Fibre Glast Developments Corporation.
| Available Properties |
- Solids Content
- Brookfield Viscosity
- Flash Point
- Cure Time
- Gel Time
- Maximum Exotherm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|