Fibre Glast 83 Waxed Polyester Laminating Resin
Subcategory: Polyester, TS; Thermoset
Material Notes: Description: #83 Waxed Polyester Laminating Resin is a prepromoted, thixotropic general purpose resin. #83 contains styrene wax for low styrene emissions and to prevent air inhibition. #83 is a waxed resin for laminating thin fiberglass skins on plywood, or for general purpose fiberglass repairs. The wax in the resin will prevent surface tackiness even when applied in thin coats. Sand off the wax layer before painting or secondary bonding.
Performance:- High thixotropic index to prevent draining in vertical surfaces
- Low viscosity for fast wet out
- Styrene suppressed
Suggested Uses:#83 Polyester Molding Resin can be used for hand lay-up or spray-up for general fiberglass reinforced plastics applications. Information provided by Fibre Glast Developments Corporation.
| Available Properties |
- Solids Content
- Brookfield Viscosity
- Flash Point
- Cure Time
- Gel Time
- Maximum Exotherm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|