Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties)

 

Subcategory: Polyester, TS; Thermoset; Polymer

Material Notes:
Description:

#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 permits fast wet-out in spray or hand laminates. Its 225°F service temperature also resists exotherm and post cure problems. Properly fabricated parts may be used in food service applications. #90 is a pre-promoted, thixotropic, corrosion and temperature-resistant Isophthalic polyester resin. This versatile product features a high molecular weight and crosslink density and offers good corrosion resistance in a variety of aqueous and acidic media. The performance of #90 has been proven by over 30 years of successful service.

Features:

  • High molecular weight Isophthalic polymer
  • Contains no esterification catalyst
  • Chemical components listed under FDA 177.2420 Title 21
  • Laminates based on #90 can meet BS 6920 requirements
  • Laminates can meet MIL-R-7575C Grade A and B with Class 0 and 3 Electrical Properties
  • Manufactured using statistical controls in ISO-9002 certified plants

Benefits:
  • Corrosion resistance, Strength, Toughness
  • Superior corrosion and blister resistance
  • Can be used in food and beverage contact application
  • Approved for use in military applications
  • Consistent batch to batch performance

Properties are listed for 1/8" Laminate, 4 plies of 1.5 oz/ft2 chopped strand mat. Glass content: 35% by weight: Thickness 0.090", at Room Temperature of 77°F

Information provided by Fibre Glast Developments Corporation.

Available Properties
  • Hardness, Barcol
  • Tensile Strength @ Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Compressive Yield Strength
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。