Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties)
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: Description:
#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 permits fast wet-out in spray or hand laminates. Its 225°F service temperature also resists exotherm and post cure problems. Properly fabricated parts may be used in food service applications. #90 is a pre-promoted, thixotropic, corrosion and temperature-resistant Isophthalic polyester resin. This versatile product features a high molecular weight and crosslink density and offers good corrosion resistance in a variety of aqueous and acidic media. The performance of #90 has been proven by over 30 years of successful service.
Features:- High molecular weight Isophthalic polymer
- Contains no esterification catalyst
- Chemical components listed under FDA 177.2420 Title 21
- Laminates based on #90 can meet BS 6920 requirements
- Laminates can meet MIL-R-7575C Grade A and B with Class 0 and 3 Electrical Properties
- Manufactured using statistical controls in ISO-9002 certified plants
Benefits:- Corrosion resistance, Strength, Toughness
- Superior corrosion and blister resistance
- Can be used in food and beverage contact application
- Approved for use in military applications
- Consistent batch to batch performance
Properties are listed for 1/8" Laminate, 4 plies of 1.5 oz/ft2 chopped strand mat. Glass content: 35% by weight: Thickness 0.090", at Room Temperature of 77°F Information provided by Fibre Glast Developments Corporation.
| Available Properties |
- Hardness, Barcol
- Tensile Strength @ Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Yield Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|