Fibre Glast 99 Clear Polyester Casting Resin
Subcategory: Polyester, TS; Thermoset
Material Notes: Description:
#99 Clear Casting Resin is ideal for poured castings. Larger castings have been achieved through multiple pours and slight catalyst adjustments. It may be used with colored pigments for opaque castings. The resin exhibits extremely low shrinkage when catalyzed at 1/2% MEKP. #99 is a low viscosity, low reactivity, orthophthalic polyester. It is prepromoted for curing with various methyl ethyl ketone peroxides (MEKPs) #69.
Features:- Low shrinkage
- Low viscosity
- UV Stabilized
- Specially promoted
Benefits:- Minimal warping
- Outstanding air release
- Meets California Rule 50 and SCAQMD 1162
- Resists yellowing
- Water white when cured
- Designed for small or large castings
Properties are typical for 1/8" Clear Casting at room temperature of 77°F Suggested Uses:Decorative castings, tabletops, art objects and biological encapsulations. Information provided by Fibre Glast Developments Corporation.
| Available Properties |
- Hardness, Barcol
- Tensile Strength @ Break
- Flexural Strength
- Maximum Service Temperature, Air
- Gel Time
- Maximum Exotherm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|