Total Petrochemicals Polystyrene 500
Subcategory: Polystyrene; Thermoplastic; Polymer
Key Words: High melt, easy flow, crystal
Material Notes: Polystyrene 500 is a high melt, easy flow crystal polystyrene for fast cycle injection molding. The high flow characteristics of this material make it easy to fill thin parts. 500 is utilized in products such as cutlery, tumblers, and containers. Other features are excellent clarity and FDA compliance. Information provided by Total Petrochemicals, Inc.
| Available Properties |
- Melt Flow
- Tensile Strength @ Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Maximum Service Temperature, Air
- Vicat Softening Point
- Process
|
|
|
|