Total Petrochemicals Polystyrene 830
Subcategory: Polystyrene; Thermoplastic; Polymer
Key Words: High melt flow, high impact
Material Notes: Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The material is targeted for large parts, thin wall parts or molds with complex runner and gate systems. Information provided by Total Petrochemicals, Inc.
| Available Properties |
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Falling Dart Impact
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Vicat Softening Point
- Gloss
- Process
|
|
|
|