Total Petrochemicals Polystyrene 935E
Subcategory: Polystyrene; Thermoplastic; Polymer
Key Words: Super high impact, toughness
Material Notes: Polystyrene 935E is a super high impact polystyrene exhibiting exceptional toughness for sheet and thermoforming applications.This polymer is an excellent choice for cups, food packaging, custom sheet and coextrusion applications when extremely high ductility is crucial. Information provided by Total Petrochemicals, Inc.
| Available Properties |
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Falling Dart Impact
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Vicat Softening Point
- Gloss
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|