Total Petrochemicals Polystyrene 960E
Subcategory: Polystyrene; Thermoplastic; Polymer
Key Words: High impact, resistance to fats and oils
Material Notes: Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids and containers for salad dressings, gravies, and high fat dairy products. Information provided by Total Petrochemicals, Inc.