Total Petrochemicals Polystyrene 965E
Subcategory: Polystyrene; Thermoplastic; Polymer
Key Words: High impact strength
Material Notes: Polystyrene 965E is a high-impact polystyrene. The extruder will see that 965E produces sheet with a dull matte finish and superior wetting tension to meet the printers needs.965E is specially designed for lithographic printing sheet. Information provided by Total Petrochemicals, Inc.
| Available Properties |
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Falling Dart Impact
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Vicat Softening Point
- Gloss
- Process
|
|
|
|