Total 3365 Polypropylene, Extrusion Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Homopolymer extrusion grade for water quench slit film Low Water Carryover - Fina 3365 exhibits excellent low water carryover which allows extrusion at maximum line speeds. High Purity - Low catalyst residues in FINA 3365 allow extended processing runs without screen pack pluggage. FDA - Fina 3365 complies with all applicable FDA regulations for food contact applications. Recommended Applications FINA 3365 is recommended for water quench slit films and monofilaments for carpet backing, rope, and cordage products. Processing - FINA 3365 processes on conventional extrusion equipment with typical melt temperatures of 400-500°F (204-260°C). Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tenacity
- Modulus of Elasticity
- Flexural Modulus
- Melting Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|