Total 3564 Polypropylene, Extrusion Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Homopolymer fiber grade for staple fiber and multifilament yarns Fading Resistance - FINA 3564 is formulated to resist gas fading while maintaining excellent processing stability. Process Stability - FINA 3564 features excellent processability and the good physical properties necessary for fibers and multifilaments. FDA - FINA 3564 complies with all applicable FDA regulations for food contact applications. Recommended Applications - FINA 3564 is recommended for staple fibers and bulk continuous filament (BCF) yarns. Processing - FINA 3564 resin processes on conventional extrusion equipment with typical melt temperatures of 400-500°F (204-260°C). Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tenacity
- Modulus of Elasticity
- Flexural Modulus
- Melting Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|