Total 3569 Polypropylene, Extrusion Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Homopolymer extrusion grade for slit film and fibrillated tapes Process Stability - FINA 3569 is formulated to be compatible with UV and pigment concentrates. FDA - FINA 3569 complies with all applicable FDA regulations and may be used under those provisions for food contact applications. Recommended Applications - FINA 3569 is recommended for high-speed slit film, monofilament and fibrillated tape applications where higher flow may be beneficial. Processing - FINA 3569 processes on conventional extrusion equipment with typical melt temperatures of 400-500°F (204-260°C). Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tenacity
- Modulus of Elasticity
- Flexural Modulus
- Melting Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|