Total 3629 Polypropylene, Injection Molding Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: LTHA injection molding homopolymer LTHA - FINA 3629 is engineered with an LTHA additive system that gives excellent leach resistance in hot/wet environments that contain bleach and laundry detergents. UL Rating - FINA 3629 has a UL rating at 120oC (248oF). FDA - FINA 3629 complies with all applicable FDA regulations for food contact applications. Recommended Applications - FINA 3629 is recommended for appliance parts and is particularly suited for parts that are exposed to a hot/wet environment such as: washing machine, dishwasher and coffee machine parts. Processing - FINA 3629 resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (200-232°C) Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|