Total 3868 Polypropylene, Extrusion Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Controlled rheology grade homopolymer for spunbond nonwoven fabrics Process Stability - FINA 3868 features excellent processability and low smoke characteristics for spunbond manufacturing. FDA - FINA 3868 complies with all applicable FDA regulations for food contact applications. Recommended Applications - FINA 3868 is recommended for spunbond nonwoven fabric and high speed melt spinning applications. Processing - FINA 3868 resin processes on conventional extrusion equipment with typical melt temperatures of 400-500°F (204- 260°C) Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tenacity
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Melting Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,