Total 8453 Polypropylene, Random Copolymer Extrusion Grade
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Random copolymer extrusion grade Clarity/Impact - the random copolymer structure of FINA 8453 improves its clarity and impact resistance over conventional homopolymer films. Heat Sealable - The reduced melting point of FINA 8453 makes it suitable as a heat seal layer for oriented films. FDA - FINA 8453 complies with all applicable FDA regulations for food contact applications. Recommended Applications - FINA 8453 is a medium ethylene content propylene copolymer product appropriate for use in a variety of applications that require improved clarity, applications that require improved clarity, flexibility, and impact strength properties or as a heat seal layer in co-extruded oriented films. Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Elongation at Break, MD
- Secant Modulus
- Seal Strength
- Melting Point
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|