Total 3373AA Polypropylene, Oriented Film Extrusion Grade
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: Homopolymer film grade Low Residuals - Fina 3373AA utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity. Slip/Antiblock - Fina 3373AA is modified with slip and antiblock additives. FDA - Fina 3373AA complies with all applicable FDA regulations and may be used under these provisions for food contact packaging. Recommended Applications - Fina 3373AA is recommended in orientation processes for manufacture of packaging tapes and films. Processing - Fina 3373AA resin processes on cast and oriented film extrusion equipment with typical melt temperatures of 450°F-525°F (232°C-274°C). Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Melting Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|