Total 3463V Polypropylene, Extrusion Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: UV Homopolymer extrusion grade for water quench slit film. Fiber UV stability 1200 hours per ASTM G-26. High Purity - Low catalyst residues in FINA 3463V allow extended processing runs without screen pack pluggage. FDA - FINA 3463V complies with all applicable FDA regulations for food contact applications. Recommended Applications - FINA 3463V is recommended for water quench slit films and monofilaments for carpet backing, rope, and cordage products requiring significant UV stability. Processing - FINA 3463V processes on conventional extrusion equipment with typical melt temperatures of 400-500°F (204-260°C). Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tenacity
- Modulus of Elasticity
- Flexural Modulus
- Melting Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|