Total 3720WZ Polypropylene, Injection Molding Grade
Subcategory: Polypropylene; Thermoplastic
Close Analogs: Total Petrochemicals now includes former Fina and Atofina plastics product lines.
Material Notes: High flow reactor injection molding homopolymer High Flow - FINA 3720WZ has high flow characteristics that result in ease of filling thin wall parts. Nucleation - FINA 3720WZ is nucleated to provide fast cycle time and improved contact clarity in thin wall, multi-cavity molds. Antistat - FINA 3720WZ contains an antistat that will help protect molded parts from dust accumulation. FDA - FINA 3720WZ complies with all applicable FDA regulations for food contact applications. Recommended Applications - FINA 3720WZ is recommended for caps, closures, and thin wall containers. Processing - FINA 3720WZ resin processes on conventional injection molding equipment with typical melt temperatures of 380-450°F (200-232°C) Data provided by the manufacturer, Total Petrochemicals.
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|